From the quality point of view, whether the product has achieved positive vulcanization, the manifestation is under-sulfur or over-sulfur. If the vulcanization is not handled properly by production, the performance of the product will not meet the standard, the wall thickness of the hose will be uneven, and the inner rubber layer will have a great impact.
If the steel wire braided or steel wire wound high-pressure hose is not in accordance with the production process, and the braiding angle does not reach 54 degrees and 44 minutes, the steel wire braiding is too tight or too loose, which will cause the product to deform during use. The poor air tightness of the inner rubber layer will easily allow the medium to enter the steel wire layer, resulting in insufficient adhesion between the steel wire layer and the rubber layer. Poor air tightness of the cover will cause the steel wire to corrode.